1、High Thermal Conductivity

2、Outstanding Corrosion Resistance
|
Corrosive medium |
Temperature(°C) |
Corrosion Rate(mg/cm2•Y) |
|
98% H2SO4 |
100 |
0.98 |
|
54% HF |
25 |
0.06 |
|
50% NaOH |
100 |
1.25 |
|
45% KOH |
100 |
0.04 |
|
70% HNO3 |
86 |
0.04 |
|
37% HCl |
25 |
0.07 |
|
10% HF & HNO3 |
25 |
0.05 |
|
10% HF & HNO3 |
120 |
1.25 |
3、Excellent Thermal & Mechanical
|
Testing Item |
Test results |
|
Bulk Density |
3.12 g/cm3 |
|
Bending strength |
400 MPa |
|
Anti Static Strength |
20 MPa |
|
Elastic modulus |
410 GPa |
|
Fracture Toughness |
3.80 MPa·m1/2 |
|
Thermal Conductivity |
140 W/m·K |
|
Thermal Expansion Coefficient |
4.66(RT-1000°C)10-6/K |
4、Health, Safety, Environment
Click:6796Degree